(TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为
宋芊汀1,2, 徐映坤1, 徐坚1()
Dry-Sliding Wear Behavior of (TiZrNbTa)90Mo10 High-Entropy Alloy Against Al2O3
SONG Qianting1,2, XU Yingkun1, XU Jian1()

图11. 在干摩擦条件下与TiZrNbTaMo-HEA和Ti6Al4V合金对磨后,Al2O3对磨球的体积损失与载荷之间的关系及与合金体积损失之间的关系

Fig.11. Volume loss vs applied loading for counterpart Al2O3 ball (a), and the relationships in volume loss between counterpart ball and the TiZrNbTaMo-HEA and Ti6Al4V alloy (b)