[an error occurred while processing this directive]
(TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为
宋芊汀1,2, 徐映坤1, 徐坚1()
Dry-Sliding Wear Behavior of (TiZrNbTa)90Mo10 High-Entropy Alloy Against Al2O3
SONG Qianting1,2, XU Yingkun1, XU Jian1()

图10. 在2、10和20 N载荷下,与TiZrNbTaMo-HEA对磨后,Al2O3球表面磨损区域的SEM像

Fig.10. SEM images (a, d, g) and corresponding high magnified images (b, c, e, f, h, i) taken from worn surface on counterpart Al2O3 ball subjected to dry sliding against TiZrNbTaMo-HEA under 2 N (a~c), 10 N (d~f) and 20 N (g~i)