[an error occurred while processing this directive]
(TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为
宋芊汀1,2, 徐映坤1, 徐坚1()
Dry-Sliding Wear Behavior of (TiZrNbTa)90Mo10 High-Entropy Alloy Against Al2O3
SONG Qianting1,2, XU Yingkun1, XU Jian1()

图7. 在2、10、20 N载荷下,TiZrNbTaMo-HEA与Al2O3球对磨3600 s后,试样表面磨痕区域的SEM像

Fig.7. SEM images (a, d, g), and corresponding high magnified images of areas I (b, e, h) and areas II (c, f, i) taken from wear track on worn surface of TiZrNbTaMo-HEA subjected to reciprocal dry sliding against Al2O3 ball under 2 N (a~c), 10 N (d~f) and 20 N (g~i) for 3600 s