(TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为
宋芊汀1,2, 徐映坤1, 徐坚1()
Dry-Sliding Wear Behavior of (TiZrNbTa)90Mo10 High-Entropy Alloy Against Al2O3
SONG Qianting1,2, XU Yingkun1, XU Jian1()

图6. 在干摩擦条件下,TiZrNbTaMo-HEA、Ti6Al4V、Co28Cr6Mo合金与Al2O3球往复式对磨3600 s后,表面磨痕的宽度和深度随载荷的变化

Fig.6. Dependence of width (a) and depth (b) in wear-track profile on applied loading for TiZrNbTaMo-HEA, Ti6Al4V and Co28Cr6Mo alloys subjected to reciprocal dry sliding against Al2O3 ball for 3600 s