(TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为
宋芊汀1,2, 徐映坤1, 徐坚1()
Dry-Sliding Wear Behavior of (TiZrNbTa)90Mo10 High-Entropy Alloy Against Al2O3
SONG Qianting1,2, XU Yingkun1, XU Jian1()

图5. 在不同干摩擦载荷下,TiZrNbTaMo-HEA、Ti6Al4V、Co28Cr6Mo合金与Al2O3球往复式对磨3600 s后,试样表面磨痕中心区域横截面沿纵深方向的二维轮廓线

Fig.5. 2D depth profiles of cross-section in central area for wear tracks on surface for TiZrNbTaMo-HEA (a), Ti6Al4V (b) and Co28Cr6Mo (c) alloys subjected to reciprocal dry sliding against Al2O3 ball for 3600 s under different loadings
Color online