[an error occurred while processing this directive]
(TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为
宋芊汀1,2, 徐映坤1, 徐坚1()
Dry-Sliding Wear Behavior of (TiZrNbTa)90Mo10 High-Entropy Alloy Against Al2O3
SONG Qianting1,2, XU Yingkun1, XU Jian1()

图4. 在不同干摩擦载荷下,TiZrNbTaMo-HEA与Al2O3球往复式对磨3600 s后试样表面磨痕的三维激光测量显微镜照片

Fig.4. 3D measuring laser microscope images for wear track on worn surface of TiZrNbTaMo-HEA subjected to reciprocal dry sliding against Al2O3 ball for 3600 s under different loadings
Color online
(a) 2 N (b) 5 N (c) 10 N (d) 20 N