(TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为
|
|
Dry-Sliding Wear Behavior of (TiZrNbTa)90Mo10 High-Entropy Alloy Against Al2O3
|
|
图2. 干摩擦条件下TiZrNbTaMo-HEA、Ti6Al4V、Co28Cr6Mo合金与Al2O3球对磨的f与载荷之间的关系 |
Fig.2. Dependence of f on applied loading for TiZrNb-TaMo-HEA, Ti6Al4V and Co28Cr6Mo alloys against Al2O3 ball under dry sliding condition |
![]() |