(TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为
宋芊汀1,2, 徐映坤1, 徐坚1()
Dry-Sliding Wear Behavior of (TiZrNbTa)90Mo10 High-Entropy Alloy Against Al2O3
SONG Qianting1,2, XU Yingkun1, XU Jian1()

图1. 在不同干摩擦载荷条件下,TiZrNbTaMo-HEA、Ti6Al4V、Co28Cr6Mo 3种合金与Al2O3对磨的摩擦系数(f)随时间变化曲线

Fig.1. Evolutions of coefficient of friction (f) with time for TiZrNbTaMo-HEA, Ti6Al4V and Co28Cr6Mo alloys under different loadings during dry sliding against Al2O3 ball (HEA—high entropy alloy)
Color online
(a) 2 N (b) 5 N (c) 10 N (d) 20 N