Er和Si对铝基储热合金导热系数及相变潜热的影响
朱伟强, 俞牧知, 唐旭, 陈孝阳, 许征兵, 曾建民

Effect of Er and Si on Thermal Conductivity and Latent Heat of Phase Transformation of Aluminum-Based Alloy
ZHU Weiqiang, YU Muzhi, TANG Xu, CHEN Xiaoyang, XU Zhengbing, ZENG Jianmin
表1 Al、Si、Er元素的热物性数据[26]
Table 1 Thermophysical property data of Al, Si and Er elements [26]
ElementTmMΔScp / (J·mol-1·K-1)
Kg·mol-1J·g-1·K-1Solid stateLiquid state
Al93427.00.42525.329.16
Si168528.11.06126.027.20
Er1795167.20.43828.136.60