[an error occurred while processing this directive]
Er和Si对铝基储热合金导热系数及相变潜热的影响
朱伟强1, 俞牧知1, 唐旭1, 陈孝阳1, 许征兵1,2(), 曾建民1,2
Effect of Er and Si on Thermal Conductivity and Latent Heat of Phase Transformation of Aluminum-Based Alloy
ZHU Weiqiang1, YU Muzhi1, TANG Xu1, CHEN Xiaoyang1, XU Zhengbing1,2(), ZENG Jianmin1,2

图6. 合金的导热系数随温度和Er含量变化的折线图

Fig.6. The thermal conductivity of the alloy changes with temperature and Er content(a) Al-12Si-xEr (b) Al-14Si-xEr (c) Al-16Si-xEr