Er和Si对铝基储热合金导热系数及相变潜热的影响
朱伟强1, 俞牧知1, 唐旭1, 陈孝阳1, 许征兵1,2(), 曾建民1,2
Effect of Er and Si on Thermal Conductivity and Latent Heat of Phase Transformation of Aluminum-Based Alloy
ZHU Weiqiang1, YU Muzhi1, TANG Xu1, CHEN Xiaoyang1, XU Zhengbing1,2(), ZENG Jianmin1,2

图2. Al-16Si-0.6Er合金的SEM像及EDS结果

Fig.2. SEM image (a) and EDS result (b) of Al-16Si-0.6Er alloy