Er和Si对铝基储热合金导热系数及相变潜热的影响
朱伟强1, 俞牧知1, 唐旭1, 陈孝阳1, 许征兵1,2(), 曾建民1,2
Effect of Er and Si on Thermal Conductivity and Latent Heat of Phase Transformation of Aluminum-Based Alloy
ZHU Weiqiang1, YU Muzhi1, TANG Xu1, CHEN Xiaoyang1, XU Zhengbing1,2(), ZENG Jianmin1,2

图1. Er/Al-Si合金显微组织的OM像

Fig.1. OM images of Al-14Si (a, b), Al-14Si-0.2Er (c, d), Al-14Si-0.4Er (e, f), Al-14Si-0.6Er (g, h) and Al-16Si-0.6Er (i, j)