异种金属焊接接头在热-力耦合作用下的断裂位置转移机理
李克俭1,2, 张宇1,2, 蔡志鹏1,2,3,4()
Fracture Location Shift of Dissimilar Metal Welds Under Coupled Thermal-Stress Effect
LI Kejian1,2, ZHANG Yu1,2, CAI Zhipeng1,2,3,4()

图10. HAZ断裂模式的试样在断口边缘附近的SEM像

Fig.10. Cross section SEM images of the area adjacent to facture surface of DMW failed in FGHAZ/ICHAZ (FGHAZ—fine-grained HAZ, ICHAZ—inter-critical HAZ)
(a) macroscopic image showing creep cavity (arrows)
(b) microscopic image showing creep cavity mainly initiated around coarsened carbides