形成Al2O3表层的奥氏体不锈钢加速蠕变实验研究
|
|
Investigations on the Accelerated Creep Testing of Alumina-Forming Austenitic Stainless Steel
|
|
图2. 形成Al2O3表层的奥氏体(AFA)不锈钢的XRD谱 |
Fig.2. XRD spectrum of the alumina-forming austenitic (AFA) stainless steel |
![]() |