图10. 实验用钢的冲击断口剖面形貌

Fig.10. SEM images of the cross-sectional area of the Charpy impact specimens
(a, b) as-forged (Fig.10a shows cracks initiated at the interfaces of M/A and matrix while Fig.10b shows cracks initiated within fractured M/A)(c, d) 400 ℃ (Fig.10d represents high-magnification image of the rectangular region in Fig.10c)