回火对钒钛微合金化Mn-Cr系贝氏体型非调质钢组织和性能的影响
|
|
Effects of Tempering Temperature on Microstructure and Mechanical Properties of a Mn-Cr Type Bainitic Forging Steel
|
|
图7. 实验用钢在不同状态下的冲击功 |
Fig.7. Impact absorbed energy of the tested steel under different conditions |
![]() |