图6. 实验用钢在锻态及不同回火温度下的示波冲击载荷(能量)-位移曲线

Fig.6. Variations of absorbed energy and impact load with displacement obtained in the instrumental impact tests of the tested steel under different conditions (Py—yield load, Pm—maximum impact load, Pf—brittle fracture start load, Pa—fracture arrested load, E1—elastic deformation energy, E2—plastic deformation energy, E3—crack propagation energy, E4—brittle fracture energy, E5—post-brittle fracture energy)
(a) as-forged (b) 200 ℃ (c) 400 ℃ (d) 500 ℃