回火对钒钛微合金化Mn-Cr系贝氏体型非调质钢组织和性能的影响
|
|
Effects of Tempering Temperature on Microstructure and Mechanical Properties of a Mn-Cr Type Bainitic Forging Steel
|
|
图5. 实验用钢的拉伸性能随回火温度的变化 |
Fig.5. Variations of tensile properties with tempering temperature (Rm—ultimate tensile strength, Rp0.2—yield strength, A—total elongation, Z—reduction of area) |
![]() |