Al中间层和Ni(V)过渡层对Co/Al/Cu三明治结构靶材背板组件焊接残余应力的影响
姜霖1,2, 张亮1,3, 刘志权1,2,4()
Effects of Al Interlayer and Ni(V) Transition Layer on the Welding Residual Stress of Co/Al/Cu Sandwich Target Assembly
JIANG Lin1,2, ZHANG Liang1,3, LIU Zhiquan1,2,4()

图7. 靶材背板组件残余应力分布

Fig.7. Distributions of residual stress in target assembly
Color online
(a) X component of residual stress (b) Y component of residual stress(c) Z component of residual stress (d) von Mises equivalent residual stress