[an error occurred while processing this directive]
Al中间层和Ni(V)过渡层对Co/Al/Cu三明治结构靶材背板组件焊接残余应力的影响
姜霖1,2, 张亮1,3, 刘志权1,2,4()
Effects of Al Interlayer and Ni(V) Transition Layer on the Welding Residual Stress of Co/Al/Cu Sandwich Target Assembly
JIANG Lin1,2, ZHANG Liang1,3, LIU Zhiquan1,2,4()

图6. Ni(V)过渡层对靶材背板组件残余应力影响

Fig.6. Effects of Ni(V) layer on the residual stress of target assembly
Color online
(a) just Al interlayer (b) Ni(V) (0.3 mm) at Co/Al interface (c) Ni(V) (0.3 mm) at Co/Al and Cu/Al interface