Al中间层和Ni(V)过渡层对Co/Al/Cu三明治结构靶材背板组件焊接残余应力的影响
姜霖1,2, 张亮1,3, 刘志权1,2,4()
Effects of Al Interlayer and Ni(V) Transition Layer on the Welding Residual Stress of Co/Al/Cu Sandwich Target Assembly
JIANG Lin1,2, ZHANG Liang1,3, LIU Zhiquan1,2,4()

图4. 有无Al中间层对扩散焊残余应力的影响

Fig.4. Effects of Al interlayer on the residual stress in the target assembly (Arrows indicate the positions of maximum residual stress)
Color online
(a) with Al interlayer (b) without Al interlayer