[an error occurred while processing this directive]
Al中间层和Ni(V)过渡层对Co/Al/Cu三明治结构靶材背板组件焊接残余应力的影响
姜霖1,2, 张亮1,3, 刘志权1,2,4()
Effects of Al Interlayer and Ni(V) Transition Layer on the Welding Residual Stress of Co/Al/Cu Sandwich Target Assembly
JIANG Lin1,2, ZHANG Liang1,3, LIU Zhiquan1,2,4()

图3. 切割前后靶材背板组件外形和残余应力测试点位置

Fig.3. Sample of diffusion welded target assembly with stress test points before (a) and after (b) cutting (The dimension of target assembly is shown in Table 1)