白斑缺陷对GH4586合金组织和力学性能的影响
谭海兵1, 黄烁2(), 王静1, 李姝1, 朱昌洪1, 钟燕1, 钟世林1, 何爱杰1
Influence of White Spot Defects on Microstructure and Mechanical Property of the GH4586 Alloy
TAN Haibing1, HUANG Shuo2(), WANG Jing1, LI Shu1, ZHU Changhong1, ZHONG Yan1, ZHONG Shilin1, HE Aijie1

图8. GH4586合金感应锭试样的EPMA元素面扫描分布图

Fig.8. EPMA elemental maps of vacuum induction melting (VIM) ingot sample of GH4586 alloy
Color online