白斑缺陷对GH4586合金组织和力学性能的影响
谭海兵1, 黄烁2(), 王静1, 李姝1, 朱昌洪1, 钟燕1, 钟世林1, 何爱杰1
Influence of White Spot Defects on Microstructure and Mechanical Property of the GH4586 Alloy
TAN Haibing1, HUANG Shuo2(), WANG Jing1, LI Shu1, ZHU Changhong1, ZHONG Yan1, ZHONG Shilin1, HE Aijie1

图6. 白斑缺陷拉伸试样断口形貌及纵剖面近断口处形貌

Fig.6. Typical fracture morphology (a) and the morphology of longitudinal section nearby the fracture (b) of the tensile sample with white spot defect