白斑缺陷对GH4586合金组织和力学性能的影响
谭海兵1, 黄烁2(), 王静1, 李姝1, 朱昌洪1, 钟燕1, 钟世林1, 何爱杰1
Influence of White Spot Defects on Microstructure and Mechanical Property of the GH4586 Alloy
TAN Haibing1, HUANG Shuo2(), WANG Jing1, LI Shu1, ZHU Changhong1, ZHONG Yan1, ZHONG Shilin1, HE Aijie1

图5. 对应图2d框线位置的白斑缺陷中第二相团簇的TEM像和SAED花样

Fig.5. TEM image (a) and SAED patterns of positions P1 (b), P2 (c) and P3 (d) of the precipitate clusters in white spot defect shown in the Fig.2d with the wire frame