[an error occurred while processing this directive]
白斑缺陷对GH4586合金组织和力学性能的影响
谭海兵1, 黄烁2(), 王静1, 李姝1, 朱昌洪1, 钟燕1, 钟世林1, 何爱杰1
Influence of White Spot Defects on Microstructure and Mechanical Property of the GH4586 Alloy
TAN Haibing1, HUANG Shuo2(), WANG Jing1, LI Shu1, ZHU Changhong1, ZHONG Yan1, ZHONG Shilin1, HE Aijie1

图4. 对应图2c区域白斑缺陷的EPMA元素面扫描分布图

Fig.4. EPMA elemental maps of white spot defect corresponding to Fig.2c
Color online