[an error occurred while processing this directive]
850 ℃涡轮盘用新型变形高温合金GH4975挤压棒材热变形规律研究
张勇1(), 李鑫旭1, 韦康1, 万志鹏1, 贾崇林1, 王涛1, 李钊1, 孙宇2, 梁红艳3
Hot Deformation Characteristics of Novel Wrought Superalloy GH4975 Extruded Rod Used for 850 ℃ Turbine Disc
ZHANG Yong1(), LI Xinxu1, WEI Kang1, WAN Zhipeng1, JIA Chonglin1, WANG Tao1, LI Zhao1, SUN Yu2, LIANG Hongyan3

图3. GH4975合金热变形过程中相关参数之间的关系

Fig.3. Relationships between lnε˙ and lnσ (a), lnε˙ and σ (b), lnε˙ and ln[sinh(ασ)] (c), ln[sinh(ασ)] and 1000/T (d), lnZ and ln[sinh(ασ)] (e) (ε˙—strain rate; σ—stress; α, β and A—material constants; Z—Zener-Hollomon parameter; T—temperature; n and n1—stress exponents; r2—correlation coefficient)