[an error occurred while processing this directive]
Fe(Pt, Ru)B非晶带材脱合金制备纳米多孔PtRuFe及其甲醇电催化性能
徐秀月, 李艳辉(), 张伟
Fabrication of Nanoporous PtRuFe by Dealloying Amorphous Fe(Pt, Ru)B Ribbons and Their Methanol Electrocatalytic Properties
XU Xiuyue, LI Yanhui(), ZHANG Wei

图4. Fe65Pt10-xRuxB25 (x=0~4)非晶合金带材脱合金后的纳米多孔合金在0.5 mol/L H2SO4和0.5 mol/L H2SO4+1.0 mol/L CH3OH混合溶液中的循环伏安曲线,纳米多孔合金的甲醇氧化峰值电流密度(jf)及正、反扫氧化峰电流密度比值(jf /jb)与Ru含量的关系(商用Pt/C数据绘在图中作为对比)

Fig.4. CV curves of nanoporous alloys fabricated by dealloying Fe65Pt10-xRuxB25 (x=0~4) amorphous alloy ribbons in 0.5 mol/L H2SO4 (a) and 0.5 mol/L H2SO4+1.0 mol/L CH3OH solutions (b), and peak current density in the forward scan (jf) and ratio of peak current density in the forward scan to that in the backward scan (jf /jb) as a function of Ru content (The data of Pt/C are shown for comparison) (c)