[an error occurred while processing this directive]
NaCl溶液腐蚀后304不锈钢的射流空蚀特征
刘海霞(), 陈金豪, 陈杰, 刘光磊
Characteristics of Waterjet Cavitation Erosion of 304 Stainless Steel After Corrosion in NaCl Solution
LIU Haixia(), CHEN Jinhao, CHEN Jie, LIU Guanglei

图6. 不同射流时间条件下试样表面微观组织的SEM像

Fig.6. SEM images of surface microstructures at different cavitation erosion time
(a) 60 min (b) 120 min (c) 240 min (d) 360 min