NaCl溶液腐蚀后304不锈钢的射流空蚀特征
刘海霞(), 陈金豪, 陈杰, 刘光磊
Characteristics of Waterjet Cavitation Erosion of 304 Stainless Steel After Corrosion in NaCl Solution
LIU Haixia(), CHEN Jinhao, CHEN Jie, LIU Guanglei

图5. 累积质量损失和质量损失率随空蚀时间的变化

Fig.5. Variations of cumulative mass loss and cumulative mass loss rate (ER) with cavitation erosion time (t)