碳钢在红沿河海洋工业大气环境中的初期腐蚀行为
宋学鑫1,2, 黄松鹏1,2, 汪川1, 王振尧1()
The Initial Corrosion Behavior of Carbon Steel Exposed to the Coastal-Industrial Atmosphere in Hongyanhe
SONG Xuexin1,2, HUANG Songpeng1,2, WANG Chuan1, WANG Zhenyao1()

图9. 碳钢表面腐蚀产物的相对含量与时间的关系

Fig.9. The relative amount of corrosion products formed on carbon steel surface as a function of exposure time