碳钢在红沿河海洋工业大气环境中的初期腐蚀行为
宋学鑫1,2, 黄松鹏1,2, 汪川1, 王振尧1()
The Initial Corrosion Behavior of Carbon Steel Exposed to the Coastal-Industrial Atmosphere in Hongyanhe
SONG Xuexin1,2, HUANG Songpeng1,2, WANG Chuan1, WANG Zhenyao1()

图6. 碳钢腐蚀60 d后的表面微观形貌及EDS分析

Fig.6. SEM images and EDS analyses (Insets show the corresponding high magnified images) of carbon steel exposed to the costal-industrial environment for 60 d
(a) low magnification (b) EDS of cotton balls (goethite)
(c) EDS of flowery structure (lepidocrocite) (d) EDS of cigar-shaped structure (akaganeite)