[an error occurred while processing this directive]
碳钢在红沿河海洋工业大气环境中的初期腐蚀行为
宋学鑫1,2, 黄松鹏1,2, 汪川1, 王振尧1()
The Initial Corrosion Behavior of Carbon Steel Exposed to the Coastal-Industrial Atmosphere in Hongyanhe
SONG Xuexin1,2, HUANG Songpeng1,2, WANG Chuan1, WANG Zhenyao1()

图5. 碳钢腐蚀10 d后的表面微观形貌及EDS分析

Fig.5. SEM images and EDS analysis of carbon steel exposed to the costal-industrial atmospheric environment for 10 d
(a) irregular localized corrosion (b) annular structure (c) mushroom-shaped structure
(d) irregular circular area (e) EDS of irregular circular area in Fig.5d