碳钢在红沿河海洋工业大气环境中的初期腐蚀行为
宋学鑫1,2, 黄松鹏1,2, 汪川1, 王振尧1()
The Initial Corrosion Behavior of Carbon Steel Exposed to the Coastal-Industrial Atmosphere in Hongyanhe
SONG Xuexin1,2, HUANG Songpeng1,2, WANG Chuan1, WANG Zhenyao1()

图3. 碳钢腐蚀后的宏观形貌

Fig.3. The surface macro-morphologies of carbon steel exposed for 10 d (a), 20 d (b), 30 d (c), 60 d (d) and 120 d (e)
Color online