碳钢在红沿河海洋工业大气环境中的初期腐蚀行为
|
|
The Initial Corrosion Behavior of Carbon Steel Exposed to the Coastal-Industrial Atmosphere in Hongyanhe
|
|
图2. 红沿河海洋工业大气环境的温度和湿度 |
Fig.2. Temperatures and relative humidities of Hongyanhe coastal-industrial atmosphere |
![]() |