含1.4%Cu的HSLA钢的组织和力学性能
杜瑜宾, 胡小锋, 张守清, 宋元元, 姜海昌, 戎利建

Microstructure and Mechanical Properties of HSLA Steel Containing 1.4%Cu
DU Yubin, HU Xiaofeng, ZHANG Shouqing, SONG Yuanyuan, JIANG Haichang, RONG Lijian
表1 2种HSLA钢的化学成分
Table 1 Chemical compositions of two HSLA steels
SteelContentCNiMnMoCrSiSPNbCuFe
0CuMass fraciton / %0.0374.030.970.500.990.210.0050.0060.0400.010Bal.
Atomic fraction / %0.1703.890.990.291.070.420.0090.0110.0240.009Bal.
1.4CuMass fraciton / %0.0414.011.000.560.950.220.0050.0070.051.40Bal.
Atomic fraction / %0.1903.881.020.321.020.440.0090.0130.031.23Bal.