中国材料基因工程研究进展
宿彦京, 付华栋, 白洋, 姜雪, 谢建新()
Progress in Materials Genome Engineering in China
SU Yanjing, FU Huadong, BAI Yang, JIANG Xue, XIE Jianxin()

图5. 机器学习方法发现新型高强高导铜合金[39]

Fig.5. New high-strength and high-electrical conductivity copper alloys discovered by the machine learning design system (MLDS) (C2P: prediction model from composition to performance; P2C: prediction model from performance to composition)[39](a) machine learning strategy for performance-oriented alloys design(b) electrical conductivity vs ultimate tensile strength of the new copper alloys discovered by the machine learning method