外延膜的高分辨X射线衍射分析
李长记1,邹敏杰1,2,张磊1(),王元明1(),王甦程1
High-Resolution X-Ray Diffraction Analysis of Epitaxial Films
LI Changji1,ZOU Minjie1,2,ZHANG Lei1(),WANG Yuanming1(),WANG Sucheng1

图14. PbTiO3/LaAlO3外延结构中衬底PbTiO3和外延膜中畴结构的(002)衍射斑的(010)倒易空间平面图的局部图

Fig.14. Local reciprocal space mapping including (002) diffraction points from the PbTiO3/LaAlO3 epitaxial structure, where LaAlO3(002) is from LaAlO3 (A, B, C, D are from the domains in the epitaxial layer PbTiO3(002))