电弧增减材复合制造精度控制研究进展
|
|
卢振洋,田宏宇,陈树君,李方
|
Review on Precision Control Technologies of Additive Manufacturing Hybrid Subtractive Process
|
|
Zhenyang LU,Hongyu TIAN,Shujun CHEN,Fang LI
|
|
| 表1 几种常见金属增材制造技术对比 |
| Table 1 Comparisons of several additive manufacturing methods of metal material |
|
Method | Welding heat source | Material type | Working condition | Dimension | Efficiency | Forming precision | Post processing |
|---|
| SLM | Laser | Powder | Inert gas | Medium-sized | Medium-low | High | Less | | EBSM | Electron beam | Powder | Vacuum | Medium-sized | Medium-low | High | Less | | LSF | Laser | Powder | Inert gas | Medium-sized | Medium-low | High | Less | | WAAM | Welding arc | Wire | Open | Large | High | Low | More |
|
|
|