金属诱导晶化基础与应用研究进展
王祖敏1(),张安1,陈媛媛1,黄远1,王江涌2
Research Progress on Fundamentals and Applications of Metal-Induced Crystallization
WANG Zumin1(),ZHANG An1,CHEN Yuanyuan1,HUANG Yuan1,WANG Jiangyong2

图5. 金属诱导非晶Si和非晶Ge晶化过程中不同结晶行为的原位XRD观察[27]

Fig.5. In situ XRD observations of the crystallization behavior differences between a-Ge (a) and a-Si (b) during metal induced crystallization (MIC)[27]