合金元素对铝合金在泰国曼谷地区初期腐蚀行为的影响
王力1,董超芳1(),张达威1,孙晓光2,Thee Chowwanonthapunya3,满成4,肖葵1,李晓刚1()
Effect of Alloying Elements on Initial Corrosion Behavior of Aluminum Alloy in Bangkok, Thailand
WANG Li1,DONG Chaofang1(),ZHANG Dawei1,SUN Xiaoguang2,Chowwanonthapunya Thee3,MAN Cheng4,XIAO Kui1,LI Xiaogang1()

图10. Fe-Si-Al第二相的SEM像、表面EDS面扫描及SKPFM结果

Fig.10. SEM image of Fe-Si-Al (a), and EDS surface scan results of Al (b), Si (c) and Fe (d), and SKPFM result (surface potential (e), surface potential of Line 2 in Fig.10e (f))