合金元素对铝合金在泰国曼谷地区初期腐蚀行为的影响
|
|
Effect of Alloying Elements on Initial Corrosion Behavior of Aluminum Alloy in Bangkok, Thailand
|
|
图8. 5083、6063和7020铝合金点蚀形貌及面扫描结果 |
Fig.8. Pitting morphologies and surface scan results of 5083 (a), 6063 (b) and 7020 (c) Al alloys |
![]() |