[an error occurred while processing this directive]
合金元素对铝合金在泰国曼谷地区初期腐蚀行为的影响
王力1,董超芳1(),张达威1,孙晓光2,Thee Chowwanonthapunya3,满成4,肖葵1,李晓刚1()
Effect of Alloying Elements on Initial Corrosion Behavior of Aluminum Alloy in Bangkok, Thailand
WANG Li1,DONG Chaofang1(),ZHANG Dawei1,SUN Xiaoguang2,Chowwanonthapunya Thee3,MAN Cheng4,XIAO Kui1,LI Xiaogang1()

图6. EIS结果拟合电路图

Fig.6. Electrochemical equivalent circuit of EIS (Re—solution resistance, CPE1—electrochemical response of the passivation film, R1—hindrance of passivation film to ion migration, CPE2—electrochemical potential of the electric double layer, R2—corresponding charge transfer resistance, Q and n are the admittance value and fitted exponential of CPE, respectively)