[an error occurred while processing this directive]
合金元素对铝合金在泰国曼谷地区初期腐蚀行为的影响
王力1,董超芳1(),张达威1,孙晓光2,Thee Chowwanonthapunya3,满成4,肖葵1,李晓刚1()
Effect of Alloying Elements on Initial Corrosion Behavior of Aluminum Alloy in Bangkok, Thailand
WANG Li1,DONG Chaofang1(),ZHANG Dawei1,SUN Xiaoguang2,Chowwanonthapunya Thee3,MAN Cheng4,XIAO Kui1,LI Xiaogang1()

图5. 曼谷暴晒1 a后5083、6063和7020铝合金在0.1 mol/L NaCl中的电化学阻抗谱(EIS)

Fig.5. Electrochemical impedance spectroscopy (EIS, in 0.1 mol/L NaCl solution at room temperature) of 5083, 6063和7020 Al alloys exposed in Bangkok area for 1 a(a) Nyquist plot (b) Bode plot