立方晶体弹性常数和EAM/FS势函数的关系
段灵杰,刘永长()
Relationships Between Elastic Constants and EAM/FS Potential Functions for Cubic Crystals
DUAN Lingjie,LIU Yongchang()

图1. 5种典型bcc结构晶体的结合能随原子间距(utot-R)的变化曲线

Fig.1. utot-R curves for five typical bcc structure crystals (R—measurement of atomic spacing)