新型钴基高温合金多尺度设计的研究现状与展望
刘兴军1,2,3(),陈悦超3,卢勇3,韩佳甲3,许伟伟3,郭毅慧3,于金鑫3,魏振帮3,王翠萍3()
Present Research Situation and Prospect of Multi-Scale Design in Novel Co-Based Superalloys: A Review
LIU Xingjun1,2,3(),CHEN Yuechao3,LU Yong3,HAN Jiajia3,XU Weiwei3,GUO Yihui3,YU Jinxin3,WEI Zhenbang3,WANG Cuiping3()

图10. 1473 K时Co-Cr-Mo三元体系富Co侧互扩散系数(D?ii)计算值与实验值对比,及扩散路径计算值与实验值对比[97]

Fig.10. Comparisons between the calculated and measured results of main interdiffusion coef?cients (D?ii) (a) and diffusion paths (b) for the fcc Co-Cr-Mo system at 1473 K[97]