[an error occurred while processing this directive]
新型钴基高温合金多尺度设计的研究现状与展望
刘兴军1,2,3(),陈悦超3,卢勇3,韩佳甲3,许伟伟3,郭毅慧3,于金鑫3,魏振帮3,王翠萍3()
Present Research Situation and Prospect of Multi-Scale Design in Novel Co-Based Superalloys: A Review
LIU Xingjun1,2,3(),CHEN Yuechao3,LU Yong3,HAN Jiajia3,XU Weiwei3,GUO Yihui3,YU Jinxin3,WEI Zhenbang3,WANG Cuiping3()

图5. 计算的Co-10Al-10W、Co-10Al-10W-10Ni、Co-10Al-10W-20Ni和Co-10Al-10W-30Ni合金的相分数曲线

Fig.5. Calculated curves of phase fraction vs temperature in Co-10Al-10W (a), Co-10Al-10W-10Ni (b), Co-10Al-10W-20Ni (c) and Co-10Al-10W-30Ni (d) alloys