新型钴基高温合金多尺度设计的研究现状与展望
刘兴军1,2,3(),陈悦超3,卢勇3,韩佳甲3,许伟伟3,郭毅慧3,于金鑫3,魏振帮3,王翠萍3()
Present Research Situation and Prospect of Multi-Scale Design in Novel Co-Based Superalloys: A Review
LIU Xingjun1,2,3(),CHEN Yuechao3,LU Yong3,HAN Jiajia3,XU Weiwei3,GUO Yihui3,YU Jinxin3,WEI Zhenbang3,WANG Cuiping3()

图1. 过渡金属元素在fcc-Co中的扩散实验数值与多种近似拟合比较[24]

Fig.1. Comparison of diffusivities of transition metal solutes in fcc cobalt calculated using various levels of approximation against experimentally measured values (D—self-diffusion coefficient, T—temperature, v*—effective frequency)[24]