合金元素对V(110)表面O吸附影响的第一性原理研究
高翔1, 张桂凯2, 向鑫2, 罗丽珠1, 汪小琳3()
Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study
GAO Xiang1, ZHANG Guikai2, XIANG Xin2, LUO Lizhu1, WANG Xiaolin3()

图5. 清洁合金化表面的表面能随合金元素化学势的变化图

Fig.5. The relative surface energies (γRS) vs the chemical potential ΔμX (X=Al, Ti and Cr) of alloy elements for the clean V(110)-Al (a), V(110)-Ti (b) and V(110)-Cr (c) alloy surfaces