[an error occurred while processing this directive]
基于有限元分析的准晶磨料强化不锈钢表面钝化行为
陈永君1,2, 白妍1, 董闯2,3(), 解志文1, 燕峰1, 吴迪1
Passivation Behavior on the Surface of Stainless Steel Reinforced by Quasicrystal-Abrasive via Finite Element Simulation
CHEN Yongjun1,2, BAI Yan1, DONG Chuang2,3(), XIE Zhiwen1, YAN Feng1, WU Di1

图11. 不同磨料处理的不锈钢在3.5%NaCl溶液中浸泡24 h的动电位极化曲线

Fig.11. Potentiodynamic polarization curves of 304 stainless steel polished by diamond, Al2O3 and QC abrasives in neutrally aerated 3.5%NaCl solution with the immersion time of 24 h